IndraLab

Statements



sparser
"Foam VF-CAM had the highest cell density (5.97 cells per mm 2 ), while foam VF-REF exhibited the lowest cell density (1.78 cells per mm 2 )."

sparser
"The reference foam (VF-REF) showed a force drop of approximately 75.2%, while the modified foams exhibited more pronounced decreases: 79.9% for VF-CAR, 79.3% for VF-CAM, and 79.2% for VF-RAP."

sparser
"This suggests that the initial recovery kinetics (up to 80%) distinguishes the reference foam clearly from the modified ones, whereas the final stage of shape recovery (from 80% to 95%) occurs with greater variability even within the bio-based group – particularly between VF-CAR (99.9 s) and VF-CAM (78.3 s)."

sparser
"The analysis reveals a clear distinction between the reference sample (VF-REF) and the foams modified with the biopolyols, whereas the differences within the group of the modified foams (VF-CAR, VF-CAM, VF-RAP) remain relatively minor."